Silicone 23 Nov 2012 | 05:33 pm
Application: • Electric parts • Lubricants SI Glass fiber Molding properties • Drying temperature : — • Drying time ...
Silicone 23 Nov 2012 | 05:33 pm
Application: • Electric parts • Lubricants SI Glass fiber Molding properties • Drying temperature : — • Drying time ...
Urea-formaldehyde 23 Nov 2012 | 05:24 pm
Application: • Laminated sheets • Textile • Colorant • Knobs • Tableware Molding properties • Drying temperature : — • Drying time ...
Urea-formaldehyde 23 Nov 2012 | 05:24 pm
Application: • Laminated sheets • Textile • Colorant • Knobs • Tableware Molding properties • Drying temperature : — • Drying time ...
Nylon 11 . 12 - PA11.12 21 Nov 2012 | 06:59 am
Molding Properties · Drying temperature : 70~80°C · Drying time : 8~15hr · Injection forming cylinder temperature ...
Nylon • 46 - PA46 Glass Fiber 45% 21 Nov 2012 | 06:58 am
Molding Properties · Drying temperature : 80°C · Drying time : 8hr · Injection forming cylinder temperature ...
Acrylonitrile-Styrene 21 Nov 2012 | 06:57 am
Also called vinyl cyanide and propene nitrile. A liquid of the composition CH2:CHCN, boiling at 78°C, used in insecticides and for producing plastic and other chemicals. It is made by the addition of...
SAN general 21 Nov 2012 | 06:56 am
Molding Properties · Drying temperature : 85°C · Drying time : 2~4hr · Injection forming cylinder temperature ...
SAN-GF Glass fiber 20~30% 21 Nov 2012 | 06:55 am
Molding Properties · Drying temperature : 85°C · Drying time : 2~4hr · Injection forming cylinder temperature :...
Polycarbonate 21 Nov 2012 | 06:54 am
Made by reacting bisphenol and phosgene, or by reacting a polyphenol with methylene chloride and phosgene. The monomer may be OC6H4C(CH3)2C6H4OC:O. The molecular structure is in double-linked zigzag ...